Ed Thompson’s Iron Trailing Slip

Firing temperature : cone 10 | Color : brown | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

Use between 4–10% red iron oxide. Test various amounts of red iron oxide added to slip before applying to your ware. If a specific viscosity or thickness is desired, add a flocculant such as vinegar or Epsom salts. Add a deflocculant, such as Darvan 811, to increase fluidity.

This recipe was shared by Robin Hopper in the November/December 2019 issue of Pottery Making Illustrated.