Instructions

Measurements in grams. Thoroughly wet the oxides with a few drops of water before adding the wax. Mix ingredients, then pass through an 80-mesh sieve to remove lumps. Clean the sieve with hot water and dish soap immediately after using.

This recipe was shared by Marc Egan in the September/October 2020 issue of Pottery Making Illustrated.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments
  • Marie M.

    I am curious what constitutes a “liquid wax emulsion”? Is this similar to what one might use for wax resist or something completely different. Thank you!