Firing temperature : Cone 6 | Surface texture : matte | Color : medium brown | Atmosphere: Oxidation/Neutral Reduction

Published in "The Fantastical Functional Forms of Kenny Delio" by Myra Bellin, in the Feb 2007 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions