Blender Batch
Firing temperature : Cone 06-11 | Surface texture : matte to satin | Color : red | Atmosphere: Oxidation ReductionIngredients
- 800
- 400
- 0.25
Instructions
*800 mL of water is 3 cups.
**For this batch size, use a few small drops of deflocculant.
This recipe yields about 500 grams of terra sigillata.
This recipe was shared by Rhonda Willers in the February 2021 issue of Ceramics Monthly, sourced from Terra Sigillata: Contemporary Techniques by Rhonda Willers.