Firing temperature : cone 01-05 |
Surface texture : matte |
Color : white |
Atmosphere:
Oxidation
Ingredients
- 6.67
- 26.67
- 26.66
Instructions
I mix this and keep it in dry form. I mix approximately a 2:1 ratio of dry base to colored stain. This recipe originally came from a workshop taken with Lisa Orr.
This recipe was shared by Lorraine Olderman in the July/August 2019 issue of Pottery Making Illustrated.