Firing temperature : cone 10-11 | Surface texture : satin | Color : Orange | Atmosphere: Reduction Salt Soda

Click Image to Enlarge

Ingredients

Instructions

This is a flashing slip for the wood kiln.

After wadding the gallery, I place the lid on the pot and the whole piece on a bat. I spray a medium thickness of flashing slip evenly over the entire exterior. I let it dry on the bat until it is ready to load into the kiln. The soda vapors or wood ash create a glaze when they land on a piece during the firings, adding nuances of color and texture.

This recipe was shared by Arylnn Nobel in the May/June 2021 issue of Pottery Making Illustrated.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend