Bartel Vitreous Slip Base

Firing temperature : cone 04 | Surface texture : satin | Color : white | Atmosphere: Oxidation

This recipe was shared by Tom Bartel in the February 2019 issue of Ceramics Monthly.


Click Image to Enlarge

Ingredients

Instructions

This base is meant to be colored with commercial stains, not oxides.