Bandana Black Slip

Firing temperature : cone 9 | Surface texture : satin | Color : black | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

Apply the black slip fairly thin, as in the consistency of skim milk.

This recipe was shared by Jason Hartsoe in the September/October 2021 issue of Pottery Making Illustrated.