Firing temperature : Cone 06-11 | Surface texture : matte to satin | Color : red | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

*28 pounds of water is 3 1/2  gallons.

**For this batch size, use 1/4 cup of deflocculant.

This recipe yields about 2 gallons of terra sigillata.

This recipe was shared by Rhonda Willers in the February 2021 issue of Ceramics Monthly, sourced from Terra Sigillata: Contemporary Techniques by Rhonda Willers.