Wadding Recipe 2

Wadding Recipe 2

Firing temperature : cone 5–10 | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

Mix to a clay-like consistency and use to separate pots from shelf. May also be molded into disks or other shapes and placed in between pots.

This recipe was shared by Stuart Gair in the April 2021 issue of Ceramics Monthly.