Stu’s Flashing Slip

Stu's Flashing Slip

Firing temperature : cone 5–10 | Surface texture : opaque matte | Color : brown | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

Apply thin layer over buff stoneware by spraying. Results range from orange to gray to brown.

This recipe was shared by Stuart Gair in the April 2021 issue of Ceramics Monthly.