Stephen Rodriguez Shino

Firing temperature : cone 10-12 | Surface texture : glossy | Color : shino | Atmosphere: Reduction Wood

Click Image to Enlarge

Instructions

Adjust the amount of Redart for color variations. Dissolve the soda ash in 1 quart of water, then add it to the glaze. Apply thin for a metallic gold and orange with crystals. Apply thick for a creamy white that blushes orange and showcases wood-ash deposits.

This recipe was shared by Trevor Youngberg in the April 2020 issue of Ceramics Monthly.