Firing temperature : cone 010-10 | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Ingredients

Instructions

This recipe can be used at all temperatures.

Mix to clay-like consistency and use in between shelves and stilts.

This recipe was shared by Stuart Gair in the April 2021 issue of Ceramics Monthly.

 