Firing temperature : cone 11 | Surface texture : glossy to satin | Color : white | Atmosphere: Reduction Wood

Click Image to Enlarge

Instructions

Apply thick by dipping or pouring in and out if just used as liner. I fire this glaze to cone 11 in a wood kiln with heavy reduction to achieve blue hare's fur. Fly ash creates  white speckling effect.

This recipe was shared by Scott McClellan in the October 2019 issue of Ceramics Monthly.