Ceramic Recipes logo

Deboos Clear-Pale Green

Deboos Clear-Pale Green

Firing temperature : cone 10-11 | Surface texture : glossy to satin | Color : green | Atmosphere: Oxidation/Neutral Reduction

Published in "Atmospheric Recipes," in the October 2018 issue of Ceramics Monthly. This recipe has been used by Susan McKinnon.


Click Image to Enlarge

Ingredients

Instructions

Add a pinch of Epsom salts to the glaze to improve consistency. Tone will vary for each of the Mason stains (MS) with different atmospheres. In reduction, the green is brighter but in oxidation it is an olive shade. In oxidation, the blue is very pale, but in reduction the color is brighter.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend