Firing temperature : cone 10 | Surface texture : satin | Color : blue | Atmosphere: Reduction Wood

Click Image to Enlarge

Ingredients

Instructions

Mix to the consistency of creamer. If applied too thick, this glaze may bubble during the firing. Add a teaspoon of Epsom salt to help with suspension.

This recipe was shared by Lisa York in the April 2020 issue of Ceramics Monthly.