Bauer Orange Flashing Slip

Firing temperature : cone 10 | Surface texture : matte | Color : Orange | Atmosphere: Salt Soda

Published in "Bauer Orange Flashing Slip," in the October 2018 issue of Ceramics Monthly. This recipe has been used by Stephen Heywood.


Click Image to Enlarge

Ingredients

Instructions

Apply by dipping, pouring, spraying, or brushing. Apply a thin coat about the consistency of skim milk to either bone-dry greenware or bisqueware.