Surface texture : satin matte | Atmosphere: Reduction

Published in "Cone 10 Clay & Glazes" by Robert Briscoe, in the Oct 2015 issue of Ceramics Monthly.

Works best in reduction. Very nice when applied thin. When applied thick goes green. The mottled textured is lost if the ash is washed. The image shown here is the White Ash Glaze over Robert Briscoe's White Bisque Slip.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Caution: Wear gloves when working with the ash as it can be caustic. Mix all ingredients prior to adding the water.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend