Recipe Tags: Zircopax

White Slip

White Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-10

Atmosphere: Reduction, Oxidation

Surface Finish: Matte

Color: White

Matt Kelleher Gloss–Pale Blue Green

Matt Kelleher Gloss–Pale Blue Green

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 3

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Blue Low-Fire Glaze

Blue Low-Fire Glaze

2 votes, average: 2.50 out of 52 votes, average: 2.50 out of 52 votes, average: 2.50 out of 52 votes, average: 2.50 out of 52 votes, average: 2.50 out of 5 (2 votes, average: 2.50 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Glossy

Color: Blue

Glaze 5

Glaze 5

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Textured

Color: Various

Glaze 3

Glaze 3

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Textured

Color: Blue

Glaze 1

Glaze 1

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Textured

Color: Various

Stick To Anything White Slip

Stick To Anything White Slip

22 votes, average: 2.82 out of 522 votes, average: 2.82 out of 522 votes, average: 2.82 out of 522 votes, average: 2.82 out of 522 votes, average: 2.82 out of 5 (22 votes, average: 2.82 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 3–12

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Matte

Color: White

Meyers White

Meyers White

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-8

Atmosphere: Oxidation/Neutral

Vince Patelka All Temperature Slip

Vince Patelka All Temperature Slip

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-10

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Matte

Color: White, Various

Yellow Salt

Yellow Salt

2 votes, average: 5.00 out of 52 votes, average: 5.00 out of 52 votes, average: 5.00 out of 52 votes, average: 5.00 out of 52 votes, average: 5.00 out of 5 (2 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10-11

Atmosphere: Reduction, Salt, Soda

Surface Finish: Satin to glossy

Color: Yellow