Fail-Safe Oxidation Base Glaze
Firing Temperature: Cone 9-10
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Miranda Thomas Clear Transparent Glaze
Firing Temperature: Cone 9
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Matte Glaze
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Matte
Color: Cream
Dense Waxy White
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin
Color: White
Smooth and Stony Glaze
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation
Surface Finish: Satin
Color: White, Brown
P-Base (Clear Stable)
Firing Temperature: Cone 6-8
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
D-Base (Clear Runny)
Firing Temperature: Cone 6-8
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Kilauea Red
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Red
Glendale Community College Gloss
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Glossy
Color: Light blue
FA’s Crystalline Base
Firing Temperature: Cone 6
Atmosphere: Oxidation/Neutral
Surface Finish: Crystalline
Color: Various