Base Ash Glaze
Firing Temperature: Cone 9-10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Clear, Blue, Yellow
P-Base (Clear Stable)
Firing Temperature: Cone 6-8
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
D-Base (Clear Runny)
Firing Temperature: Cone 6-8
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Snow
Firing Temperature: Cone 11
Atmosphere: Reduction, Oxidation
Surface Finish: Matte to satin
Color: Green
Magnesium Matte
Firing Temperature: Cone 9-10
Atmosphere: Reduction
Surface Finish: Matte
Color: White, Gray
EM Satin Base
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Clear
Nuka
Firing Temperature: Cone 11
Atmosphere: Reduction, Wood
Surface Finish: Glossy to satin
Color: White
Magnesium Matte
Firing Temperature: Cone 11
Atmosphere: Reduction
Surface Finish: Matte to satin
Color: Light brown
AC CMB15
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Matte
Color: White
Leach White
Firing Temperature: Cone 10
Atmosphere: Reduction, Oxidation
Surface Finish: Glossy
Color: White