Dense Waxy White

Dense Waxy White

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Satin

Color: White

Bright Glaze II (blue)

Bright Glaze II (blue)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 06

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Cobalt blue

Bright Glaze II

Bright Glaze II

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 06

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Dark red

Matt Glaze – Blue

Matt Glaze – Blue

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 06

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Cobalt blue