Recipe Tags: Titanium Dioxide

Selsor Red + 2% TiO2

Selsor Red + 2% TiO2

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction

Surface Finish: Glossy

Color: Dark red

Yellow Slip

Yellow Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Glossy

Color: Medium yellow

Helmer/EPK Flashing Slip

Helmer/EPK Flashing Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10-12

Atmosphere: Reduction

Surface Finish: Matte

Selsor Red + 4% TiO2

Selsor Red + 4% TiO2

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction

Surface Finish: Matte

Color: Dark tan

VC Matte Revised

VC Matte Revised

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6-9

Atmosphere: Reduction

Surface Finish: Matte

Color: Orange-red-brown

Tilton’s Celestial Pink

Tilton’s Celestial Pink

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Pink

Strontium Crystal Magic Ver. 2

Strontium Crystal Magic Ver. 2

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Light blue

Tilton Crystalline Matte

Tilton Crystalline Matte

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Oxidation/Neutral

Surface Finish: Satin matte

Color: Light yellow

Starshine

Starshine

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Turquoise green

Strontium Crystal Magic Ver. 4

Strontium Crystal Magic Ver. 4

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Oxidation/Neutral

Surface Finish: Satin matte

Color: Cream