Recipe Tags: Titanium Dioxide

Pete’s Weathered Bronze

Pete’s Weathered Bronze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6-9

Atmosphere: Reduction, Oxidation

Surface Finish: Satin

Color: Bronze, Green

Jim’s Titanium Flashing Slip

Jim’s Titanium Flashing Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10-11

Atmosphere: Reduction, Salt, Soda

Surface Finish: Satin

Color: Amber

Pete Pinnell’s Crater Glaze

Pete Pinnell’s Crater Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Textured

Color: White

Brenda’s Titanium Slip

Brenda’s Titanium Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction, Wood

Surface Finish: Satin

Color: Orange

Nuka

Nuka

2 votes, average: 2.00 out of 52 votes, average: 2.00 out of 52 votes, average: 2.00 out of 52 votes, average: 2.00 out of 52 votes, average: 2.00 out of 5 (2 votes, average: 2.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 11

Atmosphere: Reduction, Wood

Surface Finish: Glossy to satin

Color: White

Terra Sigillata Base Recipe

Terra Sigillata Base Recipe

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-2

Atmosphere: Oxidation

Surface Finish: Satin

Color: White, Gray, Yellow green, Turquoise, Yellow

Pinnell Weathered Bronze

Pinnell Weathered Bronze

9 votes, average: 3.89 out of 59 votes, average: 3.89 out of 59 votes, average: 3.89 out of 59 votes, average: 3.89 out of 59 votes, average: 3.89 out of 5 (9 votes, average: 3.89 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Satin matte

Color: Bronze

Glaze 2

Glaze 2

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Textured

Color: Green