Recipe Tags: Strontium Carbonate

Matt Kelleher Gloss

Matt Kelleher Gloss

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 2–5

Atmosphere: Reduction, Oxidation

Surface Finish: Glossy

Color: Clear

Pete Pinnell’s Crater Glaze

Pete Pinnell’s Crater Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Textured

Color: White

Pinnell Weathered Bronze

Pinnell Weathered Bronze

9 votes, average: 3.89 out of 59 votes, average: 3.89 out of 59 votes, average: 3.89 out of 59 votes, average: 3.89 out of 59 votes, average: 3.89 out of 5 (9 votes, average: 3.89 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Satin matte

Color: Bronze

AC GG Base

AC GG Base

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Satin matte

Color: Gray

Matt Kelleher Gloss–Pale Blue Green

Matt Kelleher Gloss–Pale Blue Green

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 3

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Pale Gold Crackle Glaze

Pale Gold Crackle Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 5-6

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Gold

Faux Lead Hulk Smash Green

Faux Lead Hulk Smash Green

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Green

Faux Lead Amber

Faux Lead Amber

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Glossy

Color: Amber

Matte Turquoise

Matte Turquoise

2 votes, average: 4.50 out of 52 votes, average: 4.50 out of 52 votes, average: 4.50 out of 52 votes, average: 4.50 out of 52 votes, average: 4.50 out of 5 (2 votes, average: 4.50 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Matte

Color: Turquoise green

Forest Green Celadon

Forest Green Celadon

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Matte

Color: Dark green

Enter Your Log In Credentials