Stephen Rodriguez Shino
Firing Temperature: Cone 10-12
Atmosphere: Reduction, Wood
Surface Finish: Glossy
Color: Shino
Peach Shino
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Shino
Shino Variation (1-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Satin
Color: Brown
Sprite Bottle Green 04
Firing Temperature: Cone 04-03
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Green
Chris Clear
Firing Temperature: Cone 01-05
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear, Turquoise, Green, Blue
Avery Shino
Firing Temperature: Cone 9-13
Atmosphere: Reduction, Wood, Salt, Soda
Surface Finish: Satin to glossy
Color: Medium brown, Medium tan, Medium red, Various
K-Shino
Firing Temperature: Cone 10
Atmosphere: Reduction, Wood
Color: Shino
Oestreich Shino
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Various
Pete’s STD Shino
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Various
Will Swanson Shino
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Various