Limestone Clear
Firing Temperature: Cone 10
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Glossy
Color: Clear
Laura’s Turquoise
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Matte
Color: Turquoise blue
Lau Luster Shino
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Matte
Color: Clear
Kujaku (Peacock) Glaze, Type 2
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Turquoise blue
Kujaku (Peacock) Glaze, Type 1
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Turquoise blue
Kujaku (Peacock) Glaze
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Turquoise blue
Ketchup Red
Firing Temperature: Cone 6
Atmosphere: Oxidation/Neutral
Surface Finish: Matte
Color: Medium red
John’s Satin Blue Celadon
Firing Temperature: Cone 6
Atmosphere: Reduction
Surface Finish: Matte
Color: Dark green
John’s Red
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Matte
Color: Dark red
John’s Red
Firing Temperature: Cone 10
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Turquoise blue