Tony Hansen’s G2934—Silky Black
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Black
Tony Hansen’s G2934—Brown
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Brown
Tony Hansen’s G2934—White
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: White
White Engobe
Firing Temperature: Cone 06-02
Atmosphere: Oxidation
Surface Finish: Glossy to satin
Color: White
Iron Slip
Firing Temperature: Cone 9
Atmosphere: Reduction, Wood
Surface Finish: Matte to satin
Color: Brown
Pete’s Best Moving Clear
Firing Temperature: Cone 6-10
Atmosphere: Reduction, Oxidation
Surface Finish: Glossy
Color: Clear
Tenmoku Gold
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Glossy to satin
Color: Gold, Tenmoku
Ian’s Ash
Firing Temperature: Cone 10
Atmosphere: Oxidation
Surface Finish: Glossy to satin
Color: Amber
Slate Blue
Firing Temperature: Cone 6
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Blue
Ed Thompson’s Iron Trailing Slip
Firing Temperature: Cone 10
Atmosphere: Reduction, Oxidation
Color: Brown