Fail-Safe Oxidation Base Glaze
Firing Temperature: Cone 9-10
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Lung Chuan Celadon for Reduction Cooling
Firing Temperature: Cone 9-10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Blue
FLM Transfer Slip
Firing Temperature: Cone 9-10
Atmosphere: Reduction, Oxidation
Surface Finish: Matte to satin
Color: White
Val Cushing Floor Tile Body
Firing Temperature: Cone 6
Atmosphere: Oxidation
Color: White, Off white
Bomb-Proof White Tile Body
Firing Temperature: Cone 10
Atmosphere: Reduction, Oxidation
Color: White
Egan Gloss Base
Firing Temperature: Cone 2–3
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Ian Begg’s Clear
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Pete Pinnell’s Crater Glaze
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Textured
Color: White
Bates Clear
Firing Temperature: Cone 10
Atmosphere: Reduction, Oxidation
Surface Finish: Glossy
Color: Blue
Tony Hansen’s G2934—Silky Black
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Black