Nathan Bray’s Copper Green Glaze
Firing Temperature: Cone 04-6
Surface Finish: Glossy to satin
Color: Green
Base Ash Glaze
Firing Temperature: Cone 9-10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Clear, Blue, Yellow
Lisa Orr Light Turquoise 04
Firing Temperature: Cone 03-04
Atmosphere: Reduction
Surface Finish: Glossy
Color: Turquoise, Blue
Kilauea Red
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Red
Faux Lead Hulk Smash Green
Firing Temperature: Cone 04
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Green
Faux Lead Amber
Firing Temperature: Cone 04
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Glossy
Color: Amber
Lichen Glaze
Firing Temperature: Cone 04-6
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Textured
Color: Various
Pier Day-Glo High-Fire glaze
Firing Temperature: Cone 8-9
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Glossy
Color: Pink, Chartreuse
Base Glaze – Emerald
Firing Temperature: Cone 04-03
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Medium green
Iron Crystalline Glaze
Firing Temperature: Cone 11-12
Atmosphere: Oxidation/Neutral
Surface Finish: Satin to glossy
Color: Clear