Recipe Tags: Rutile

Bill’s Basic Liner Glaze

Bill’s Basic Liner Glaze

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-2

Atmosphere: Oxidation

Surface Finish: Glossy

Color: White

Slate Blue

Slate Blue

3 votes, average: 3.33 out of 53 votes, average: 3.33 out of 53 votes, average: 3.33 out of 53 votes, average: 3.33 out of 53 votes, average: 3.33 out of 5 (3 votes, average: 3.33 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction

Surface Finish: Glossy to satin

Color: Blue

Oriental Iron Glaze (1-F5-R9)

Oriental Iron Glaze (1-F5-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy to satin

Color: Blue, Tan

Oriental Iron Glaze (9-F4-R9)

Oriental Iron Glaze (9-F4-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Matte to satin

Color: Medium green, Tan

Shiny Flux Variation (7-F5-R9)

Shiny Flux Variation (7-F5-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction

Surface Finish: Satin

Color: Light yellow

Shiny Flux Variation (7-F5-O6)

Shiny Flux Variation (7-F5-O6)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Crystalline, Matte to satin

Color: Tan

Shiny Flux Variation (13-F4-R9)

Shiny Flux Variation (13-F4-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction

Surface Finish: Glossy to satin

Color: Blue, Purple

Base Ash Glaze

Base Ash Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9-10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Clear, Blue, Yellow

Low to Mid Clear

Low to Mid Clear

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-6

Atmosphere: Oxidation

Surface Finish: Glossy

Color: Clear

Tan-Yellow Transparent

Tan-Yellow Transparent

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Oxidation

Color: Medium tan, Light tan, Yellow

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image