Ohata Khaki

Ohata Khaki

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction, Salt, Soda

Surface Finish: Glossy

Color: Brown

Miranda Thomas Black Slip

Miranda Thomas Black Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction, Oxidation

Surface Finish: Matte

Color: Black

Miranda Thomas Jun Glaze

Miranda Thomas Jun Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Brown

Cuerda Seca Wax Recipe

Cuerda Seca Wax Recipe

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Color: Black

Iron Slip

Iron Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction, Wood

Surface Finish: Matte to satin

Color: Brown

Tenmoku Gold

Tenmoku Gold

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Glossy to satin

Color: Gold, Tenmoku

Ed Thompson’s Iron Trailing Slip

Ed Thompson’s Iron Trailing Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction, Oxidation

Color: Brown

Blue Salt

Blue Salt

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction, Wood

Surface Finish: Satin

Color: Blue

Oriental Iron Glaze (3-A6-R9)

Oriental Iron Glaze (3-A6-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy

Color: Brown

Oriental Iron Glaze (3-A5-R9)

Oriental Iron Glaze (3-A5-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy

Color: Black, Brown