Recipe Tags: Ofuyu Stone

Iraho Oxidation Glaze

Iraho Oxidation Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Oxidation/Neutral

Surface Finish: Satin matte

Color: Dark brown