Parian Test 4
Firing Temperature: Cone 9
Atmosphere: Reduction, Oxidation
Color: White
Parian Test 5
Firing Temperature: Cone 9
Atmosphere: Reduction, Oxidation
Color: White
Parian Test 6
Firing Temperature: Cone 9
Atmosphere: Reduction, Oxidation
Color: White
FLM Transfer Slip
Firing Temperature: Cone 9-10
Atmosphere: Reduction, Oxidation
Surface Finish: Matte to satin
Color: White
Val Cushing Floor Tile Body
Firing Temperature: Cone 6
Atmosphere: Oxidation
Color: White, Off white
Bates Clear
Firing Temperature: Cone 10
Atmosphere: Reduction, Oxidation
Surface Finish: Glossy
Color: Blue
P-Base (Clear Stable)
Firing Temperature: Cone 6-8
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
D-Base (Clear Runny)
Firing Temperature: Cone 6-8
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Clear Glaze
Firing Temperature: Cone 4-6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Fake Korean Celadon
Firing Temperature: Cone 5-6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Green celadon