Recipe Tags: Kona F-4 Feldspar

Bill’s Basic Liner Glaze

Bill’s Basic Liner Glaze

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-2

Atmosphere: Oxidation

Surface Finish: Glossy

Color: White

My #3 Matte

My #3 Matte

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6-7

Atmosphere: Oxidation

Surface Finish: Matte

Color: Clear

Blue Low-Fire Glaze

Blue Low-Fire Glaze

2 votes, average: 2.50 out of 52 votes, average: 2.50 out of 52 votes, average: 2.50 out of 52 votes, average: 2.50 out of 52 votes, average: 2.50 out of 5 (2 votes, average: 2.50 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Glossy

Color: Blue

Avery Shino

Avery Shino

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9-13

Atmosphere: Reduction, Wood, Salt, Soda

Surface Finish: Satin to glossy

Color: Medium brown, Medium tan, Medium red, Various

Oestreich Shino

Oestreich Shino

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Various

Pete’s STD Shino

Pete’s STD Shino

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Various

Will Swanson Shino

Will Swanson Shino

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Various

Malcom Davis Carbon-Trap Shino

Malcom Davis Carbon-Trap Shino

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Medium orange

Blue-Green/Copper Red Glaze

Blue-Green/Copper Red Glaze

4 votes, average: 4.25 out of 54 votes, average: 4.25 out of 54 votes, average: 4.25 out of 54 votes, average: 4.25 out of 54 votes, average: 4.25 out of 5 (4 votes, average: 4.25 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Glossy

Color: Medium green, Medium red

Gustin Shino #5

Gustin Shino #5

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Satin matte

Color: Medium brown

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image