Recipe Tags: Iron Chromate

Fake Korean Celadon

Fake Korean Celadon

7 votes, average: 4.57 out of 57 votes, average: 4.57 out of 57 votes, average: 4.57 out of 57 votes, average: 4.57 out of 57 votes, average: 4.57 out of 5 (7 votes, average: 4.57 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 5-6

Atmosphere: Oxidation

Surface Finish: Glossy

Color: Green celadon

Low-Fire Crackle (green)

Low-Fire Crackle (green)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Green

Dark Blue Luster

Dark Blue Luster

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 08

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Dark blue