Cone 6 Translucent Porcelain
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation
Color: White
Pale Peach Terra Sigillata
Firing Temperature: Cone 04-11
Atmosphere: Wood
Surface Finish: Satin
Color: Peach
Blue/Green V.2 Terra Sigillata
Firing Temperature: Cone 04-11
Atmosphere: Wood
Surface Finish: Satin
Color: Blue green
Blue/Green V.1 Terra Sigillata
Firing Temperature: Cone 04-11
Atmosphere: Wood
Surface Finish: Satin
Color: Blue green
Miranda Thomas White Slip
Firing Temperature: Cone 10
Atmosphere: Reduction, Oxidation
Surface Finish: Matte to satin
Color: White
Miranda Thomas Jun Glaze
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Brown
Magnesium Matte
Firing Temperature: Cone 9-10
Atmosphere: Reduction
Surface Finish: Matte
Color: White, Gray
White Slip
Firing Temperature: Cone 04-10
Atmosphere: Reduction, Oxidation
Surface Finish: Matte to satin
Color: White
Blue Celadon
Firing Temperature: Cone 11
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Blue
Turquoise Matte
Firing Temperature: Cone 6-7
Atmosphere: Oxidation
Surface Finish: Matte
Color: Turquoise