Nathan Bray’s Copper Green Glaze
Firing Temperature: Cone 04-6
Surface Finish: Glossy to satin
Color: Green
Sprite Bottle Green 04
Firing Temperature: Cone 04-03
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Green
Low to Mid Clear
Firing Temperature: Cone 04-6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Fake Korean Celadon
Firing Temperature: Cone 5-6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Green celadon
N502 Transparent and Glossy + MnO2
Firing Temperature: Cone 5
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Dark brown
N502 Transparent , Glossy + CuCo3 + TiO2
Firing Temperature: Cone 5
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Dark green
Chatterley Glaze
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Textured
Color: Gray