Odyssey Clear
Firing Temperature: Cone 4-6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Bates Clear
Firing Temperature: Cone 10
Atmosphere: Reduction, Oxidation
Surface Finish: Glossy
Color: Blue
Tenmoku Gold
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Glossy to satin
Color: Gold, Tenmoku
Slate Blue
Firing Temperature: Cone 6
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Blue
Nancy’s Pink Icing Glaze
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Pink
Leather Glaze with Red Iron Oxide
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation
Surface Finish: Satin
Color: Brown
Leather Glaze with Copper Carbonate
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation
Surface Finish: Satin
Color: Green
Leather Glaze with Cobalt Carbonate
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation
Surface Finish: Satin
Color: Lavender
Leather Glaze
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation
Surface Finish: Satin
Color: White
Snow
Firing Temperature: Cone 11
Atmosphere: Reduction, Oxidation
Surface Finish: Matte to satin
Color: Green