Recipe Tags: frit 3289 or pemco frit 626

Lana Wilson Purple Aqua

Lana Wilson Purple Aqua

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 06

Atmosphere: Oxidation/Neutral

Surface Finish: Textured

Color: Medium purple