Recipe Tags: Flint

Robbie’s Y altered

Robbie’s Y altered

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 8

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Cobalt blue

Chun Reduced

Chun Reduced

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Light blue

Purple Nuke

Purple Nuke

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Satin matte

Color: Medium blue

Copper Grape

Copper Grape

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Dark purple

Conrad Engobe

Conrad Engobe

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04, Cone 7

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: White

Magnesia Matt

Magnesia Matt

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Off white

Emmanuel Cooper Blue Crystal

Emmanuel Cooper Blue Crystal

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Medium blue

Starshine

Starshine

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Turquoise green

Mark’s Purple

Mark’s Purple

6 votes, average: 2.50 out of 56 votes, average: 2.50 out of 56 votes, average: 2.50 out of 56 votes, average: 2.50 out of 56 votes, average: 2.50 out of 5 (6 votes, average: 2.50 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Medium purple

Boysenberry

Boysenberry

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Light green