Recipe Tags: Ferro Frit 3195

LG #2 + Cobalt Carbonate

LG #2 + Cobalt Carbonate

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Surface Finish: Textured

Color: Blue

Nathan Bray’s Copper Green Glaze

Nathan Bray’s Copper Green Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-6

Surface Finish: Glossy to satin

Color: Green

Low to Mid Clear

Low to Mid Clear

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-6

Atmosphere: Oxidation

Surface Finish: Glossy

Color: Clear

High-Calcium Semi-Matte Base 2

High-Calcium Semi-Matte Base 2

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction, Oxidation

Surface Finish: Glossy

Color: Clear, Gray blue, Amber

Betty’s Bisque Slip

Betty’s Bisque Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 01-05

Atmosphere: Oxidation

Surface Finish: Matte

Color: White

Stick To Anything White Slip

Stick To Anything White Slip

23 votes, average: 2.87 out of 523 votes, average: 2.87 out of 523 votes, average: 2.87 out of 523 votes, average: 2.87 out of 523 votes, average: 2.87 out of 5 (23 votes, average: 2.87 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 3–12

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Matte

Color: White

Pier Day-Glo High-Fire glaze

Pier Day-Glo High-Fire glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 8-9

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Glossy

Color: Pink, Chartreuse

John’s 10x Series #12

John’s 10x Series #12

1 vote, average: 1.00 out of 51 vote, average: 1.00 out of 51 vote, average: 1.00 out of 51 vote, average: 1.00 out of 51 vote, average: 1.00 out of 5 (1 votes, average: 1.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Medium brown

Pete Pinnell Clear

Pete Pinnell Clear

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-2

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Clear

John’s 10x Series #11 Blue Glaze

John’s 10x Series #11 Blue Glaze

1 vote, average: 1.00 out of 51 vote, average: 1.00 out of 51 vote, average: 1.00 out of 51 vote, average: 1.00 out of 51 vote, average: 1.00 out of 5 (1 votes, average: 1.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Light blue, Dark yellow, Gray blue