EM Satin Base
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Clear
Easy E Clear
Firing Temperature: Cone 6
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Clear
Blue Low-Fire Glaze
Firing Temperature: Cone 04
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Glossy
Color: Blue
Low Fire White Engobe (Gail Kendall)
Firing Temperature: Cone 06-03
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Satin matte
Color: White
Lichen Glaze
Firing Temperature: Cone 04-6
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Textured
Color: Various
Meyers White
Firing Temperature: Cone 04-8
Atmosphere: Oxidation/Neutral
Zinc-free Clear
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Glossy
Color: Clear
Lynn Peters Majolica Overglaze Colors
Firing Temperature: Cone 03
Atmosphere: Oxidation/Neutral
Color: Various
Pottery Northwest White Slip
Firing Temperature: Cone 04-3
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Matte
Color: White
Pottery Northwest “Henna”
Firing Temperature: Cone 04-3
Atmosphere: Reduction, Oxidation/Neutral
Color: Terra cotta