Cone 6 Casting Slip
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation
Color: White
Naples-Wagner Satin Clear Cone 1–2
Firing Temperature: Cone 1–2
Atmosphere: Oxidation
Surface Finish: Satin
Color: Clear, Brown
Lisa Orr Light Turquoise 04
Firing Temperature: Cone 03-04
Atmosphere: Reduction
Surface Finish: Glossy
Color: Turquoise, Blue
Sprite Bottle Green 04
Firing Temperature: Cone 04-03
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Green
Chris Clear
Firing Temperature: Cone 01-05
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear, Turquoise, Green, Blue
Low-Fire Crackle (green)
Firing Temperature: Cone 04
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Green
Low-fire Crackle (Blue)
Firing Temperature: Cone 04
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Blue
Water Blue
Firing Temperature: Cone 6
Atmosphere: Oxidation/Neutral
Surface Finish: Matte
Color: Blue
Pale Gold Crackle Glaze
Firing Temperature: Cone 5-6
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Gold
Glaze 6
Firing Temperature: Cone 04
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Textured
Color: Various