Recipe Tags: Feldspar

Matte Flux Variation (4-D3-R9)

Matte Flux Variation (4-D3-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Color: Tan

Flux Saturation (6-E3-O6)

Flux Saturation (6-E3-O6)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Glossy to satin

Color: Purple

Shiny Flux Variation (13-F4-R9)

Shiny Flux Variation (13-F4-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction

Surface Finish: Glossy to satin

Color: Blue, Purple

Shiny Flux Variation (5-C3-R9)

Shiny Flux Variation (5-C3-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy

Color: Light brown

Shiny Flux Variation (5-C4-R9)

Shiny Flux Variation (5-C4-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy

Color: Dark green

Shiny Flux Variation (5-C2-R9)

Shiny Flux Variation (5-C2-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy to satin

Color: Cranberry red

Shiny Flux Variation (8-D5-R9)

Shiny Flux Variation (8-D5-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy

Color: Brown

Shiny Flux Variation (8-D6-R9)

Shiny Flux Variation (8-D6-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy

Color: Brown

Shiny Flux Variation (5-A1-R9)

Shiny Flux Variation (5-A1-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy to satin

Color: Orange

Shiny Flux Variation (6-A1-R9)

Shiny Flux Variation (6-A1-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Satin

Color: Orange