Vari-egated Green (Varigreen)
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Green
Opaque Matte #5
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Matte
Color: White, Blue
Ron Myers Clear
Firing Temperature: Cone 04-6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear, Red
Matt Kelleher Gloss
Firing Temperature: Cone 2–5
Atmosphere: Reduction, Oxidation
Surface Finish: Glossy
Color: Clear
Cone 6 Casting Slip
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation
Color: White
Poor Man’s Porcelain Slip
Firing Temperature: Cone 04-10
Atmosphere: Reduction, Oxidation
Color: White
Odyssey Clear
Firing Temperature: Cone 4-6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear
Naples-Wagner Satin Clear Cone 1–2
Firing Temperature: Cone 1–2
Atmosphere: Oxidation
Surface Finish: Satin
Color: Clear, Brown
Parian Test 7
Firing Temperature: Cone 9
Atmosphere: Reduction, Oxidation
Color: White
Parian Test 8
Firing Temperature: Cone 9
Atmosphere: Reduction, Oxidation
Color: White