Recipe Tags: Custer Feldspar

Leach White

Leach White

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Surface Finish: Glossy, Satin

Color: White, Light blue

Seth’s Iron-Rich Stoneware #2

Seth’s Iron-Rich Stoneware #2

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 5–7

Atmosphere: Reduction

Surface Finish: Satin

Color: Brown

Bill Kremer’s Notre Dame Class Mix

Bill Kremer’s Notre Dame Class Mix

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction, Oxidation

Surface Finish: Satin

Color: Tan, Brown

Cone 6 Casting Slip

Cone 6 Casting Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction, Oxidation

Color: White

Parian Test 7

Parian Test 7

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction, Oxidation

Color: White

Parian Test 8

Parian Test 8

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction, Oxidation

Color: White

Parian Test 9

Parian Test 9

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction, Oxidation

Color: White

Fail-Safe Oxidation Base Glaze

Fail-Safe Oxidation Base Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9-10

Atmosphere: Oxidation

Surface Finish: Glossy

Color: Clear

Lung Chuan Celadon for Reduction Cooling

Lung Chuan Celadon for Reduction Cooling

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9-10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Blue

Ian’s Ash

Ian’s Ash

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Oxidation

Surface Finish: Glossy to satin

Color: Amber