Recipe Tags: Cullet (from Budweiser bottles)

Brisco Alkaline Glaze

Brisco Alkaline Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Glossy

Color: Medium brown