Tenmoku Gold
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Glossy to satin
Color: Gold, Tenmoku
Ian’s Ash
Firing Temperature: Cone 10
Atmosphere: Oxidation
Surface Finish: Glossy to satin
Color: Amber
Oriental Iron Glaze (3-A6-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Brown
Oriental Iron Glaze (3-A5-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Black, Brown
Oriental Iron Glaze (3-A4-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Brown
Oriental Iron Oxide (3-A3-R9)
Firing Temperature: Cone 9
Surface Finish: Glossy
Color: Brown
Oriental Iron Glaze (3-A1-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Blue
Oriental Iron Glaze (1-F5-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Blue, Tan
Oriental Iron Glaze (29-B1-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Blue
Oriental Iron Glaze (11-B1-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Blue