Vari-egated Green (Varigreen)
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Green
Reynolds Green Metal Patina
Firing Temperature: Cone 6
Surface Finish: Satin
Color: Black
Slate Blue
Firing Temperature: Cone 6
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Blue
Nathan Bray’s Copper Green Glaze
Firing Temperature: Cone 04-6
Surface Finish: Glossy to satin
Color: Green
Oribe Green
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Green, Blue
Oriental Iron Glaze (19-C1-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Red
Oriental Iron Glaze (19-C3-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Dark red
Flux Saturation (5-C1-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Blue
Flux Saturation (4-C1-O6)
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Glossy to satin
Color: Light blue
Flux Saturation (5-C3-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Blue